Polymer Property : Flexural Modulus = 1746 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 12.04 GPa
1746 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON RX05489 PA 66
LNP* STAT-KON* RX05489 is a compound based on Nylon 66 resin containing 10% Carbon Fiber, 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear..