Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 12.04 GPa | 1746 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON RX05489 PA 66 LNP* STAT-KON* RX05489 is a compound based on Nylon 66 resin containing 10% Carbon Fiber, 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear.. |