Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.206 GPa | 174.9 ksi | ASTM D790A |
Polymer Industries Densetec PP Copolymer Sheet Polymer Industries’ Densetec Copolymer Propylene differs from the Densetec Homopolymer Polypropylene by virtue of an additional monomer in the product, thus making it a copolymer material. This is .. |
|||
Flexural Modulus | 1.206 GPa | 174.9 ksi | |
CMW® THERMKON® 68 Tungsten Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |