Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Industries Densetec PP Copolymer Sheet

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Polymer Industries
Trade Name Densetec
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polymer Industries Densetec PP Copolymer Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polymer Industries’ Densetec Copolymer Propylene differs from the Densetec Homopolymer Polypropylene by virtue of an additional monomer in the product, thus making it a copolymer material. This is achieved by adding ethylene to the material during the polymerization process. This helps the material achieve higher impact strength and toughness characteristics even at very low temperatures.Information provided by Polymer Industries.
Physical Properties Metric English Comments
Density 0.901 g/cc
0.0326 lb/in³
ASTM D792
Melt Index of Compound 0.70 g/10 min
0.70 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 78
78
ASTM D785
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Elongation at Yield 13 %
13 %
ASTM D638
Flexural Modulus 1.206 GPa
174.9 ksi
ASTM D790A
Izod Impact, Notched NB
NB
ASTM D256
Falling Dart Impact 29.0 J
21.4 ft-lb
-29°C; Private Lab
Thermal Properties Metric English Comments
Melting Point 162 °C
324 °F
Private Lab