Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.40 - 17.7 GPa | 203 - 2560 ksi | Average value: 2.33 GPa Grade Count:82 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |