Polymer Property : Flexural Modulus = 1595.1 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 10.998 GPa
1595.1 ksi
ASTM D790
Aclo Accutech Polycarbonate POL050G40L Glass Reinforced
Flexural Modulus 10.998 GPa
1595.1 ksi
ASTM D790
Aclo Accutech Polycarbonate POL051G40L Glass Reinforced