Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.998 GPa | 1595.1 ksi | ASTM D790 |
Aclo Accutech Polycarbonate POL050G40L Glass Reinforced |
|||
Flexural Modulus | 10.998 GPa | 1595.1 ksi | ASTM D790 |
Aclo Accutech Polycarbonate POL051G40L Glass Reinforced |