Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.092 GPa | 158.4 ksi | 1% Secant; 12.5 mm/min; ASTM D790 |
LyondellBasell Alathon® H5112 High Density Polyethylene, Injection Molding Grade ALATHON H5112 is a medium-molecular-weight-distribution resin with balanced impact/ESCR and high flow characteristics. Typical applications include housewares, food containers, pail handles and toys.. |