Polymer Property : Flexural Modulus = 1564 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 10.78 GPa
1564 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP QF008 PA 6/10 (Asia Pacific)
LNP* Thermocomp* QF008 is a compound based on Nylon 6/10 resin containing Glass Fiber.
Flexural Modulus 10.78 GPa
1564 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP QF008 PA6.10
LNP* THERMOCOMP* QF008 is a compound based on Nylon 6/10 resin containing 40% Glass Fiber.
Flexural Modulus 10.78 GPa
1564 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Thermocomp QF008R PA 6/10
LNP* Thermocomp* QF008R is a compound based on Nylon 6/10 containing Glass Fiber. Characteristics of this grade are: Easy Release.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 10.78 GPa
1564 ksi
ISO 178
SABIC Innovative Plastics LNP Thermocomp QF008S PA 6/10
LNP* Thermocomp* QF008S is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas ..
Flexural Modulus 10.78 GPa
1564 ksi
ASTM D790
SABIC Innovative Plastics NORYL GTX APS440 PPE+PPS (Asia Pacific)
PPE+PPS, GF40%, FR V-0
Flexural Modulus 10.78 GPa
1564 ksi
ASTM D790
SABIC Innovative Plastics NORYL APS440 PPE+PPS (Asia Pacific)
Flexural Modulus 10.78 GPa
1564 ksi
ISO 178
SABIC Innovative Plastics LNP Thermocomp QF008S PA 6/10 (Asia Pacific)
LNP* Thermocomp* QF008S is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Paci..