Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.00 - 10.6 GPa | 580 - 1540 ksi | Average value: 5.66 GPa Grade Count:8 |
Overview of materials for Glass Reinforced, Modified SMA This property data is a summary of similar materials in the MatWeb database for the category "Glass Reinforced, Modified SMA". Each property range of values reported is minimum and maximum values of.. |
|||
Flexural Modulus | 3.46 - 10.62 GPa @Temperature -40.0 - 200 °C |
502 - 1540 ksi @Temperature -40.0 - 392 °F |
Average value: 5.77 GPa Grade Count:2 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |