Polymer Property : Flexural Modulus = 153.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.055 GPa
153.0 ksi
ASTM D790
Chevron Phillips K-Resin® KK38 Styrene-Butadiene Copolymer, Sheet Grade
Styrene-Butadiene CopolymerCustomer Benefits: KK38 is an improved extrusion grade SBC designed specifically for superior performance in blends with general purpose polystyrene. It is easily process..