Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.055 GPa | 153.0 ksi | ASTM D790 |
Chevron Phillips K-Resin® KK38 Styrene-Butadiene Copolymer, Sheet Grade Styrene-Butadiene CopolymerCustomer Benefits: KK38 is an improved extrusion grade SBC designed specifically for superior performance in blends with general purpose polystyrene. It is easily process.. |