Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 15.59 GPa | 2261 ksi | ASTM D790 |
PlastiComp Complet® LGF60-PA66 MT 60% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |