Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 15.53 GPa | 2252 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DX04489C PC LNP STAT-KON* DX04489C is a high modulus compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Con.. |
|||
Flexural Modulus | 15.53 GPa | 2252 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP VC006 SUPER TOUGH NYLON LNP* THERMOTUF* VC006 is a compound based on Super Tough Nylon resin containing 30% Carbon Fiber. Added features of this material include: High Impact, Electrically Conductive. |
|||
Flexural Modulus | 15.53 GPa | 2252 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOTUF VC006 Super Tough PA 6/6 LNP* THERMOTUF* VC006 is a compound based on Super Tough Nylon 6/6 resin containing Carbon Fiber. Added features of this material include: High Impact. |