Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.910 - 147 GPa | 132 - 21300 ksi | Average value: 13.8 GPa Grade Count:136 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |