Polymer Property : Flexural Modulus = 14.0653 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.40 - 14.0653 GPa

@Temperature -40.0 - 120 °C
203 - 2040.03 ksi

@Temperature -40.0 - 248 °F
Average value: 6.70 GPa Grade Count:3
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum..