Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 13.79 GPa | 2000 ksi | ASTM D-790 |
PlastiComp Velocity® LGF50-PA6 High Flow Nylon 6, 50% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |