Polymer Property : Flexural Modulus = 125 GPa
Polymer Property :
Flexural Modulus =
125 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus
125
GPa
18100
ksi
Longitudinal
Goodfellow Carbon/Epoxy Composite Rod
Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow.