Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.8273 GPa | 120.0 ksi | 1% Secant; ASTM D 790 |
Chevron Phillips LX8119 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear copolymer; ASTM D4976 Classification: PE 233, A 56700Characteristics: warp resistant, excellent impact strength, excellent ESCR, moderate shrinkage resistanceApplications: seats, .. |