Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips LX8119 HDPE Injection Molding Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips LX8119 HDPE Injection Molding Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: linear copolymer; ASTM D4976 Classification: PE 233, A 56700Characteristics: warp resistant, excellent impact strength, excellent ESCR, moderate shrinkage resistanceApplications: seats, containers, food containers, agricultural applications, industrial applicationsInformation provided by Chevron Phillips Chemical Company.
Physical Properties Metric English Comments
Density 0.945 g/cc
0.0341 lb/in³
ASTM D4883
Apparent Bulk Density 0.590 g/cc
0.0213 lb/in³
ASTM D1895
Environmental Stress Crack Resistance 40 hour
40 hour
ASTM D1693B
Melt Flow 6.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.4 MPa
3390 psi
ASTM D638
Elongation at Break >= 1000 %
>= 1000 %
ASTM D638
Flexural Modulus 0.8273 GPa
120.0 ksi
1% Secant; ASTM D 790
Thermal Properties Metric English Comments
Vicat Softening Point 122 °C
252 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746