Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 11.83 GPa | 1716 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Verton RX93407D PA 66 LNP* Verton* RX93407D is a compound based on Nylon 66 resin.This data was supplied by SABIC-IP for the Americas region. |