Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 11.26 GPa | 1633 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DF008ER PC LNP THERMOCOMP* DF008ER is a compound based on Polycarbonate resin containing 40% Glass Fiber. Added features include: Easy Molding, Mold Release. |
|||
Flexural Modulus | 11.26 GPa | 1633 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon RE003 PA 66 LNP STAT-KON* RE003 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americ.. |
|||
Flexural Modulus | 11.26 GPa | 1633 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DF008ERH PC LNP THERMOCOMP* DF008ERH is a compound based on Polycarbonate resin containing 40% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Healthcare. |