Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.00 - 7.40 GPa | 580 - 1070 ksi | Average value: 5.96 GPa Grade Count:7 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Flexural Modulus | 2.55 - 7.35 GPa | 370 - 1070 ksi | Average value: 3.94 GPa Grade Count:23 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Flexural Modulus | 2.30 - 7.35 GPa | 334 - 1070 ksi | Average value: 3.53 GPa Grade Count:135 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Flexural Modulus | 2.26 - 7.40 GPa | 328 - 1070 ksi | Average value: 4.50 GPa Grade Count:21 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |