Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.7419 GPa | 107.6 ksi | ASTM D790 |
Quadrant EPP TIVAR® MD UHMW-PE, FDA Metal Detectable (ASTM Product Data Sheet) Meets FDA and USDA guidelines; 3-A Dairy-approved (natural) Reduces noise Self-lubricating Chemical-, corrosion- and wear-resistant No moisture absorption Non-toxic, low-friction surface Meets ASTM.. |