Polymer Property : Flexural Modulus = 0.7419 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.7419 GPa
107.6 ksi
ASTM D790
Quadrant EPP TIVAR® MD UHMW-PE, FDA Metal Detectable (ASTM Product Data Sheet)
Meets FDA and USDA guidelines; 3-A Dairy-approved (natural) Reduces noise Self-lubricating Chemical-, corrosion- and wear-resistant No moisture absorption Non-toxic, low-friction surface Meets ASTM..