Flexural Modulus 1.978 GPa
286.9 ksi
ASTM D790
RedEye On Demand Clear PolyJet™ FC720 for Rapid Prototyping
Clear PolyJet Resin (FC720) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Clear PolyJet Resin material offer..