Mechanical Properties Metric English Comments
Flexural Modulus 1.78 GPa
258 ksi
ASTM D790
Polymer Resources PPX-GP4-WR Modified-PPO, General Purpose, Wear Resistant
Modified-Polyphenylene Oxide, General Purpose, Wear Resistant, 215F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s..
Flexural Modulus 1.78 GPa
258 ksi
ASTM D790
Polymer Resources TP-IM1 Polybutylene Terephthalate, Low Temperature Impact Modified
Polybutylene Terephthalate, Low Temperature Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
Flexural Modulus 1.78 GPa
258 ksi
ASTM D790
LNP Stat-Kon® PDX-S-90398 Polyamide 12, Stainless Steel Fiber  (discontinued **)
Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades..
Flexural Modulus 1.78 GPa
258 ksi
2 mm/min, 64mm span; ISO 178
SABIC Innovative Plastics SABIC PPCOMPOUND 8620A PP
SABIC® PPcompound 8620A is a mineral filled, impact modified polypropylene TPO. It was originally designed for painted automotive bumper fascia applications where a combination of good flow, hig..
Flexural Modulus 1.78 GPa
258 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Xenoy® 6620U PBT+PC
PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance.
Flexural Modulus 1.78 GPa
258 ksi
ASTM D790
Styrolution Terluran® EHI-4 NR ABS Extrusion Application
Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Flexural Modulus 1.78 GPa
258 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP MF003AS PP
LNP* THERMOCOMP* MF003AS is a compound based on Polypropylene containing 15% Glass Fiber. Characteristics of this grade are: Heat Stabilized.
Flexural Modulus 1.78 GPa
258 ksi
ISO 178
Polyplastics Duranex® CA7200NX Polybutylene Terephthalate (PBT), Antistatic
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Flexural Modulus 1.78 GPa
258 ksi
ASTM D790
Polymer Resources PPX-GP4-WR Modified PPO, Wear Resistant with HDT of 215 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Flexural Modulus 1.78 GPa
258 ksi
Tangent, chs 0.05 in/min; ASTM D790
Diamond Polymers ABS/PC 9801
Description: Injection Molding Grade, High Impact, High HeatInformation provided by Diamond Polymers, Inc.