Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.0345 GPa | 150.04 ksi | Method 1, Proc. B; ASTM D-790-95 |
Multibase Multi-Flex® TPO D-6206 This TPO product was developed for facia applications exhibiting adhesion for current automotive paint systems.Data provided by Multibase. |