Mechanical Properties Metric English Comments
Flexural Modulus 0.6998 - 1.03 GPa
101.5 - 150 ksi
ASTM D790
Buckeye Polymers BP FLEX D6020-08 BLK Thermoplastic Polyolefin
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist..