Buckeye Polymers BP FLEX D6020-08 BLK Thermoplastic Polyolefin

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Buckeye Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Buckeye Polymers BP FLEX D6020-08 BLK Thermoplastic Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resistanceGood UV resistanceLow densityWide service range from -20°C to 120°CAppearance: BlackForms: Gala cut round pelletsProcessing Method: Injection MoldingInformation Provided by Buckeye Polymers, Inc.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0095 - 0.012 cm/cm
0.0095 - 0.012 in/in
ASTM D955
Melt Flow 6.0 - 12 g/10 min
6.0 - 12 g/10 min
ASTM D1238
Ash <= 5.0 %
<= 5.0 %
ASTM D5630
Mechanical Properties Metric English Comments
Flexural Modulus 0.6998 - 1.03 GPa
101.5 - 150 ksi
ASTM D790
Izod Impact, Notched >= 5.34 J/cm
>= 10.0 ft-lb/in
ASTM D256
Gardner Impact >= 339 J
>= 250 ft-lb
ASTM D5420