Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.00689 GPa | 1.00 ksi | ASTM D790 |
Lubrizol Estane® ALR E72A Thermoplastic Polyurethane Type: Estane® ALR E72A is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corpor.. |