Material Notes:
Type: Estane® ALR E72A is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm
0.0080 - 0.012 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 72
72
ASTM D2240
Tensile Strength, Ultimate 40.0 MPa
5800 psi
ASTM D412
Elongation at Break 660 %
660 %
ASTM D412
100% Modulus 0.00207 GPa
0.300 ksi
ASTM D412
200% Modulus 0.00345 GPa
0.500 ksi
ASTM D412
300% Modulus 0.00552 GPa
0.800 ksi
ASTM D412
Flexural Modulus 0.00689 GPa
1.00 ksi
ASTM D790