Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.00585 GPa | 0.848 ksi | 1% Secant; ASTM D790 |
Multibase Multi-Flex® A 8406 A Natural TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |