Multibase Multi-Flex® A 8406 A Natural TPE Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Multibase
Trade Name Multi-Flex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® A 8406 A Natural TPE Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM 792
Melt Flow 9.55 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.55 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 86
86
10 seconds; ASTM D2240
Tensile Strength, Ultimate 8.41 MPa
1220 psi
ASTM D638
Elongation at Break 820 %
820 %
ASTM D638
Flexural Modulus 0.00585 GPa
0.848 ksi
1% Secant; ASTM D790
Tear Strength 47.3 kN/m
270 pli
ASTM D624