Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.590 - 0.840 GPa | 85.6 - 122 ksi | Average value: 0.694 GPa Grade Count:9 |
Overview of materials for Medium Density Polyethylene (MDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max.. |