Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.590 GPa | 85.6 ksi | ASTM D790 |
NOVA Chemicals Sclair® 35BP HDPE Extrusion Resin, 2.2% Carbon Black Filled
(discontinued **) Features: Excellent ESCR, medium molecular weight, good processability, excellent long term thermal stability, good chemical resistance, excellent UV stability.Applications: Extrusion on to metal pi.. |
|||
Flexural Modulus | 0.590 - 0.810 GPa | 85.6 - 117 ksi | Average value: 0.673 GPa Grade Count:8 |
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m.. |
|||
Flexural Modulus | 0.590 GPa | 85.6 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem MB 0434 LS-L MDPE IPQ employs Spherilene technology from Basell in the production of MDPE. The raw materials, which are supplied by COPESUL, are pre-treated and fed into gas-phase reactors, where medium density polye.. |
|||
Flexural Modulus | 0.590 GPa | 85.6 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem MB 0435 MDPE IPQ employs Spherilene technology from Basell in the production of MDPE. The raw materials, which are supplied by COPESUL, are pre-treated and fed into gas-phase reactors, where medium density polye.. |
|||
Flexural Modulus | 0.590 GPa | 85.6 ksi | ISO 178 |
Borealis Casico™ FR4805 Non Halogen Flame Retardant Compound for Sheathing Energy Cables Casico FR4805 is a thermoplastic, non-halogen containing natural jacketing compound. It combines high mechanical strength and toughness with flame retardancy. The composition of Casico FR4805 is b.. |
|||
Flexural Modulus | 0.590 GPa | 85.6 ksi | ASTM D790 |
Covestro Bayflex® 180 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o.. |
|||
Flexural Modulus | 0.590 GPa | 85.6 ksi | ASTM D790 |
Asahi Glass Fluon® P-65P PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Flexural Modulus | 0.590 GPa | 85.6 ksi | ASTM D790 |
Asahi Glass Fluon® P-805UP PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Flexural Modulus | 0.590 GPa | 85.6 ksi | ASTM D790 |
NOVA Chemicals Sclair® 35BPM MDPE Extrusion Resin, 2.2% Carbon Black Filled
(discontinued **) Features: Excellent ESCR, medium molecular weight, good processability, excellent long term thermal stability, good chemical resistance, excellent UV stability.Applications: Extrusion on to metal pi.. |
|||
Flexural Modulus | 0.590 - 0.840 GPa | 85.6 - 122 ksi | Average value: 0.694 GPa Grade Count:9 |
Overview of materials for Medium Density Polyethylene (MDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max.. |