Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.705 GPa | 102 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 396 Ionomer DescriptionFormion® FI 3936is a 3% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, and impact. Formion F1 396U is UV stabilized to exceed .. |
|||
Flexural Modulus | 0.705 GPa | 102 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 396 Ionomer DescriptionFormion® FI 3936is a 3% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, and impact. Formion F1 396U is UV stabilized to exceed .. |
|||
Flexural Modulus | 0.705 GPa | 102 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 396 Ionomer DescriptionFormion® FI 3936is a 3% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, and impact. Formion F1 396U is UV stabilized to exceed .. |
|||
Flexural Modulus | 0.705 GPa | 102 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 396 Ionomer DescriptionFormion® FI 3936is a 3% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, and impact. Formion F1 396U is UV stabilized to exceed .. |
|||
Flexural Modulus | 0.705 GPa | 102 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 396 Ionomer DescriptionFormion® FI 3936is a 3% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, and impact. Formion F1 396U is UV stabilized to exceed .. |
|||
Flexural Modulus | 0.705 GPa | 102 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 396 Ionomer DescriptionFormion® FI 3936is a 3% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, and impact. Formion F1 396U is UV stabilized to exceed .. |
|||
Flexural Modulus | 0.705 GPa | 102 ksi | 0.05 in/min; ISO 178 |
CTC X-PRO CTC PP 2019 Polypropylene Impact Copolymer X-PRO PP 2019 is a high impact, polypropylene copolymer. It has automotive and industrial general purpose applications.Data provided by Composite Technologies (CTC). |