A. Schulman FORMION™ FI 396 Ionomer

Category Polymer , Thermoplastic , Ionomer
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman FORMION™ FI 396 Ionomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionFormion® FI 3936is a 3% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, and impact. Formion F1 396U is UV stabilized to exceed SAE J1960 2500 kj/m2 automotive performance criteria, and is targeted for non painted, mold-in-color, exterior or interior appearance applications.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ISO 1183/1
Linear Mold Shrinkage 0.0060 - 0.010 cm/cm

@Thickness 3.20 mm
0.0060 - 0.010 in/in

@Thickness 0.126 in
72 hr; ISO 294
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
15 sec delay; ISO 868
Tensile Strength, Ultimate 19.0 MPa
2760 psi
at max load; ISO 527
Elongation at Break 375 %
375 %
ISO 527
Flexural Modulus 0.705 GPa
102 ksi
Tangent; ISO 178
Izod Impact, Notched (ISO) 40.0 kJ/m²
19.0 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 52.0 °C

@Thickness 3.20 mm
126 °F

@Thickness 0.126 in
ISO 75