Polymer Property : Flexural Modulus = 0.510 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.510 GPa
74.0 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE G 7940 GRAPHITE
Ash is 7.3%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Flexural Modulus 0.510 GPa
74.0 ksi
1.3 mm/min, 50 mm span; ASTM D790
Ovation Polymers Nemcon™ E HDPE 11000 HDPE
HDPE-ESD Range Conductivity with improved processability and UV resistance.Information provided by Ovation Polymers
Flexural Modulus 0.510 GPa
74.0 ksi
ASTM D790
PolyOne Maxxam™ FR PE 152 Polyethylene, Unspecified (PE, Unspecified)
Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V..