Multibase Multi-Flex® TPE G 7940 GRAPHITE

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE G 7940 GRAPHITE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ash is 7.3%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.9616 g/cc
0.03474 lb/in³
ASTM D792
Melt Flow 3.1 g/10 min
3.1 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
10 sec; ASTM D-2240
Tensile Strength, Ultimate 13.7 MPa
1990 psi
ASTM D412
Elongation at Break 597 %
597 %
ASTM D412
Flexural Modulus 0.510 GPa
74.0 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 112.43 kN/m
641.53 pli
ASTM D624