Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.365 GPa | 52.9 ksi | ASTM D790 |
PolyOne Gravi-Tech™ GRV-UR-045-SS-W Black Polyurethane, Unspecified (PUR, Unspecified) Information provided by PolyOne |
|||
Flexural Modulus | 0.365 GPa | 53.0 ksi | 1% Secant; ASTM D790 |
LyondellBasell Petrothene® PR92735 Linear Low Density Polyethylene ApplicationsPETROTHENE PR 92735 is a high molecular weight, linear low density-based compound designed for cable jacketing. PR 92735 contains a nominal carbon black content of 2.6% and antioxidant .. |
|||
Flexural Modulus | 0.365 GPa | 53.0 ksi | ASTM D790 |
Teknor Apex Telcar® TL-1000-95 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Flexural Modulus | 0.365 GPa | 53.0 ksi | tangent, 1.3 mm/min; ASTM D790 |
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl.. |
|||
Flexural Modulus | 0.365 GPa @Temperature -20.0 °C |
52.9 ksi @Temperature -4.00 °F |
ASTM D790 |
DuPont Elvax® 670 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Flexural Modulus | 0.365 GPa | 53.0 ksi | tangent, 1.3 mm/min; ASTM D790 |
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl.. |
|||
Flexural Modulus | 0.365 GPa | 53.0 ksi | tangent, 1.3 mm/min; ASTM D790 |
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl.. |
|||
Flexural Modulus | 0.365 GPa | 53.0 ksi | tangent, 1.3 mm/min; ASTM D790 |
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl.. |
|||
Flexural Modulus | 0.365 GPa | 53.0 ksi | tangent, 1.3 mm/min; ASTM D790 |
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl.. |
|||
Flexural Modulus | 0.365 GPa | 53.0 ksi | tangent, 1.3 mm/min; ASTM D790 |
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl.. |
|||
Flexural Modulus | 0.365 GPa | 52.9 ksi | XD; ASTM D790 |