PolyOne Gravi-Tech™ GRV-UR-045-SS-W Black Polyurethane, Unspecified (PUR, Unspecified)

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer PolyOne Corporation
Trade Name Gravi-Tech™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Gravi-Tech™ GRV-UR-045-SS-W Black Polyurethane, Unspecified (PUR, Unspecified).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 4.49 g/cc
4.49 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0060 - 0.010 cm/cm
0.0060 - 0.010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
10 sec; ASTM D2240
60
60
ASTM D2240
Tensile Stress 8.69 MPa

@Strain 100 %
1260 psi

@Strain 100 %
ASTM D412
Elongation at Break 100 %
100 %
ASTM D412
Flexural Yield Strength 12.4 MPa
1800 psi
13 mm/min; ASTM D790
Flexural Modulus 0.365 GPa
52.9 ksi
ASTM D790
Izod Impact, Notched 2.10 J/cm

@Thickness 3.18 mm
3.93 ft-lb/in

@Thickness 0.125 in
ASTM D256
Descriptive Properties Value Comments
Features High Density
Non-Toxic
Forms Pellets
Generic Material PUR, Unspecified
Generic Name Polyurethane, Unspecified (PUR, Unspecified)
Processing Method Injection Molding
Regional Availability North America
Uses Industrial Applications
Projectiles
Sporting Goods
Weighting & Balancing