Polymer Property : Flexural Modulus = 0.141 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.141 GPa
20.5 ksi
Dow AFFINITY™ PL 1840 Polyolefin Plastomer
AFFINITY® PL 1840 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide blown film products with low temperature sealability, excellent puncture resistance, outstanding blown f..