Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 0.0931 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.0931 GPa
13.5 ksi
ASTM D790
LyondellBasell Microthene® F FE53200 Ethylene Vinyl Acetate Copolymer
General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene..
Flexural Modulus 0.0931 GPa
13.5 ksi
ASTM D790
LyondellBasell Microthene® G MU76300 Ethylene Vinyl Acetate Copolymer
General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop..
Copyright © lookpolymers.com All Rights Reserved