Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Microthene® G MU76300 Ethylene Vinyl Acetate Copolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate; Molded/Extruded
Manufacturer LyondellBasell (former Equistar)
Trade Name Microthene® G
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Microthene® G MU76300 Ethylene Vinyl Acetate Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique properties of a polyolefin resin with a small ground particle size. Contact your Equistar sales and/or technical service representative for more information and specific recommendations for your application.Process TechniquesThe microfine size and irregular shape of Microthene G powders facilitate dispersibility with other components. Specific suggestions can be made only when equipment, materials, process parameters and conditions of use are known. Contact your Equistar technical representative for more information. Regulatory StatusMicrothene powders comply with certain Food and Drug Administration regulations, which may or may not permit their contact with food. Specific limitations or conditions of use may apply. Contact your Equistar Regulatory Affairs representative for more information. This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.927 g/cc
0.0335 lb/in³
ASTM D1505
Particle Mesh Size 35 Mesh
35 Mesh
Irregular shape. ETM = Equistar Test Method; ETM Malvern
Melt Flow 11 g/10 min
11 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 38
38
ASTM D2240
Tensile Strength at Break 11.7 MPa
1700 psi
ASTM D638
Elongation at Break 675 %
675 %
ASTM D638
Flexural Modulus 0.0931 GPa
13.5 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 96.0 °C
205 °F
ASTM D3418
Vicat Softening Point 75.0 °C
167 °F
ASTM D1525
Brittleness Temperature -76.0 °C
-105 °F
ASTM D746