Polymer Property : Flexural Modulus = 0.0303 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.0303 GPa
4.39 ksi
ASTM D790
DuPont™ Surlyn® 8320 Ionomer Resin, Sodium
Surlyn® 8320 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. This very low modulus sod..