Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 0.0200 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.0200 GPa
2.90 ksi
1% Secant, ASTM D790
ExxonMobil Escorene® LD-769 High EVA Compounding Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymer designed for high filler acceptance. Compounds produced from this resin have excellent flexibility and toughness.Appl..
Flexural Modulus 0.0200 GPa
2.90 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCD825 PPE-TPE (Asia Pacific)
Flexible, very low-migration, halogen-free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame retardant performance capable of meeting UL VW-1 re..
Flexural Modulus 0.0200 GPa
2.90 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCD825 PPE-TPE (Asia Pacific)
Flexible, very low-migration, halogen-free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame retardant performance capable of meeting UL VW-1 re..
Flexural Modulus 0.0200 GPa
2.90 ksi
1% secant; ASTM D790
ExxonMobil Escorene® UL 8705 Adhesive Application Resin
Escorene Ultra UL 8705 is a relatively low viscosity, 27.6% vinyl acetate copolymer specifically tailored for enhanced modulus/tensile performance at the same viscosity of similar materials. It has ..
Flexural Modulus 0.0200 GPa
2.90 ksi
ASTM D638
Arkema Group LOTRYL® 20 MA 08 Copolymer Ethylene - Methyl Acrylate
LOTRYL® 20 MA 08 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 20 MA 08 is a polyme..
Flexural Modulus 0.0200 GPa
2.90 ksi
ASTM D638
Arkema Group LOTADER® 4403 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 4403 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure autoclave process. LOTADER 4403 is a versatile adhesive for extrusion lamination, de..
Flexural Modulus 0.0200 GPa
2.90 ksi
ASTM D638
Arkema Group LOTADER® 4503 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 4503 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process.LOTADER 4503 is a versatile adhesive for extrusion lamination, des..
Flexural Modulus 0.0200 GPa
2.90 ksi
ASTM D638
Arkema Group LOTRYL® 20 MBG 08 Copolymer Ethylene - Methyl Acrylate
LOTRYL® 20MBG08 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 20 MBG 08 is a polyme..
Copyright © lookpolymers.com All Rights Reserved