Mechanical Properties Metric English Comments
Flexural Modulus 0.00500 - 0.0427 GPa
0.725 - 6.20 ksi
Average value: 0.0222 GPa Grade Count:5
Overview of materials for Ethylene Acrylic Acid
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri..
Flexural Modulus 0.00500 GPa
0.725 ksi
ASTM D638
Arkema Group LOTRYL® 37 EH 175 Copolymer Ethylene - 2-Ethylhexyl Acrylate
LOTRYL® 37EH175 is a random copolymer of Ethylene and 2-Ethylhexyl Acrylate, prepared by the high pressure polymerization process. LOTRYL® 37EH175 is particularly recommended for the formulation o..