Polymer Property : Flexural Modulus = 0.00207 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.00207 GPa
0.300 ksi
ASTM D790
Teknor Apex TEKRON® 4000-25 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Flexural Modulus 0.00207 - 2.26 GPa
0.300 - 327 ksi
Average value: 0.274 GPa Grade Count:120
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and..