Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex TEKRON® 4000-25 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Teknor Apex Company
Trade Name TEKRON®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex TEKRON® 4000-25 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
+/- 0.02; ASTM D792
Melt Flow 4.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 25
25
ASTM D2240
Tensile Strength, Yield 5.45 MPa
790 psi
ASTM D412
Elongation at Break 840 %
840 %
ASTM D412
100% Modulus 0.000345 GPa
0.0500 ksi
ASTM D412
Flexural Modulus 0.00207 GPa
0.300 ksi
ASTM D790
Tear Strength 13.1 kN/m
75.0 pli
Die C; ASTM D1004
Copyright © lookpolymers.com All Rights Reserved